We aim to find out quality disfigurement from the production and supply the best service to domestic and overseas customers wholeheartedly for high quality film for food packing , polyamide film , balloon lighting film , We warmly welcome all standpoint inquiries from home and abroad to cooperate with us, and anticipate your correspondence.
Factory For Thermal Bopa Film - MESIM BOPA With Balanced Physical Properties And Converting – Changshu Detail:

Features Benefits
● Good oxygen/aroma barrier
● Outstanding isotropy performance in printing and retort
● Longer shelf life and better freshness
● Excellent converting performance and registration accuracy
● Excellent tensile strength, anti-punch and anti-impact properties
● High flex-crack resistance
● Wide temperature range in application
● Excellent transparency and gloss
● Capacity with excellent packaging safety to apply to heavy packaging, sharp and rigid products.
● Minimum distortion after retort

SHA can be used for producing the high-grade packaging within12 colors, sealing width ≤10cm and needs printing registration. It is not easy to warp and curl after 125℃ retorting. It’s recommended to be used for non-heavy packaging products with single bag capacity less than 2kg, for example, retort pouch and cup lid with delicate patterns.

Thickness /μm Width/mm Treatment Retortability Printability
15 300-2100 single/both side corona ≤121℃ ≤12 colors

Notice: retortability and printability are depending on customers’ lamination and printing processing condition.

Performance BOPP BOPET BOPA
Puncture Resistance
Flex-crack Resistance ×
Impact Resistance
Gases Barrier ×
Humidity Barrier ×
High Temperature Resistance
Low Temperature Resistance ×

bad×      normal△      quite good○      excellent◎

1
2
2121

The Small Dot/Shallow Net Lost

Print dots are missing or missed in the shallow position of the printed pattern (generally less than 30% of the dot, serious in 50% of the dot will also appear).

Causes:

Ink fineness is not enough, resulting in some large particles of ink cannot be filled to the network of shallow holes;

● Ink concentration is too thick, resulting in poor printing, the formation of dot hollowing;

● Scraper pressure is too large resulting in small amount of ink, ink supply is uneven, resulting in the loss of small dots;

● The use of too much quick-drying solvent, resulting in the ink drying up in the net hole and unable to attach to the film during the transfer process of the shallow net part;

● Printing speed is too slow, in the ink drying up in the net hole during the transfer process;

● Film surface is too rough; the underlying ink is not smooth.

Related Suggestions:

✔ Choose fineness ≤15μm ink;

✔ Appropriate dilute ink viscosity;

✔ The doctor blade should be adjusted to just scrape the ink, not to put too much pressure;

✔ Use less quick-drying solvent to adjust the drying speed of ink on the plate roller;

✔ Try to ensure that the speed of more than 160m/min printing.


Product detail pictures:

Factory For Thermal Bopa Film -
 MESIM BOPA With Balanced Physical Properties And Converting  – Changshu detail pictures


Related Product Guide:

We insist on offering premium quality manufacturing with superior business concept, honest product sales as well as finest and fast assistance. it will bring you not only the good quality product or service and huge profit, but the most significant is to occupy the endless market for Factory For Thermal Bopa Film - MESIM BOPA With Balanced Physical Properties And Converting – Changshu , The product will supply to all over the world, such as: Mozambique , Nicaragua , Sao Paulo , Look forward to the future, we will focus more on the brand building and promotion . And in the process of our brand global strategic layout we welcome more and more partners join us, work together with us based on mutual benefit. Let's develop market by fully utilizing our comprehensive advantages and strive for building.
  • The supplier abide the theory of "quality the basic, trust the first and management the advanced" so that they can ensure a reliable product quality and stable customers.
    5 Stars By Elma from Bangalore - 2017.04.08 14:55
    The factory technical staff not only have high level of technology, their English level is also very good, this is a great help to technology communication.
    5 Stars By jari dedenroth from Argentina - 2017.08.21 14:13
    Write your message here and send it to us